Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.01 GPa | 146 ksi | X, Y direction; ASTM D638 |
Rogers Corporation RT/duroid® 6202 High Frequency Laminate Features:Low loss for excellent high frequency performanceTight dielectric constant and thickness controlExcellent electrical and mechanical propertiesExtremely low thermal coefficient of dielectric.. |
|||
Tensile Modulus | 1.01 GPa | 146 ksi | X, Y direction; ASTM D638 |
Rogers Corporation RT/duroid® 6202PR High Frequency Laminate Features:Low loss for excellent high frequency performanceTight dielectric constant and thickness controlExcellent electrical and mechanical propertiesExtremely low thermal coefficient of dielectric.. |
|||
Tensile Modulus | 1.01 GPa | 146 ksi | 1mm/min |
Eastman Tenite 264-16 CAB Cellulose Acetate Butyrate
(discontinued **) 16% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Tensile Modulus | 1.01 GPa | 146 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP 2X00858 FP-F (FEP) LNP* THERMOCOMP* 2X00858 is a compound based on FEP resin containing proprietary fillers. |
|||
Tensile Modulus | 1.01 GPa | 146 ksi | Secant; ISO 527-2 |
ExxonMobil Exxtral™ BNU 013 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good impact resistance, high stiffness, good scratch and good surface finishing designed for automotive interior ap.. |