Mechanical Properties Metric English Comments
Tensile Modulus 0.100 GPa
14.5 ksi
1mm/min; DIN 53457
Advanced Elastomer Systems VistaFlex® 715-N Thermoplastic Rubber  (discontinued **)
Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f..
Tensile Modulus 0.100 GPa

@Temperature 23.0 °C
14.5 ksi

@Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Hytrel® HTR8685 BK022A TPC-ET  (Unverified Data**)
Hytrel® HTR8685 BK022A is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal hardness of 44D, is pigmented black with fine particle size carbon black,..
Tensile Modulus 0.100 GPa
14.5 ksi
LATI Latigray 47/1-01 CX/45 PP Copolymer
Radiopaque compound based on Polypropylene copolymer (PPc). Special mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati ..
Tensile Modulus 0.100 - 0.300 GPa

@Thickness 2.00 mm
14.5 - 43.5 ksi

@Thickness 0.0787 in
1.0 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 32008 Polyvinylidene Fluoride (PVDF)
Solef® 32008 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional ..
Tensile Modulus 0.100 GPa
14.5 ksi
ISO 527-1/-2
DSM Arnitel® EM460 46 Shore D, Injection Molding or Extrusion Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Modulus 0.100 GPa
14.5 ksi
ISO 527-1/-2
DSM Arnitel® EM460 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Modulus 0.100 GPa
14.5 ksi
ISO 527-1/-2
DSM Arnitel® PL420-H Injection Molding Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Modulus 0.100 GPa
14.5 ksi
ISO 527-1/-2
DSM Arnitel® PL420-H Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Modulus 0.100 GPa
14.5 ksi
ISO 527-1/-2
DuPont Performance Polymers Hytrel® HTR8685 BK022A Polyester Elastomer TPC-ET  (Unverified Data**)
44 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Hytrel HTR8685 BK022A is designed for blow molding or processing techniques requi..
Tensile Modulus 0.100 GPa
14.5 ksi
cond.; ISO 527
Azoty Tarnow™ Tarnamid® T-29 MS Polyamide 6 - Natural
Medium-high viscosity extrusion grade for mono or multilayer blown film, including biaxial oriented films, also for production of monofilament; can be used for injection molding and compounding.For ..
Tensile Modulus 0.100 GPa
14.5 ksi
cond.; ISO 527
Azoty Tarnow™ Tarnamid® T-29 Polyamide 6 - Natural
Medium-high viscosity extrusion grade for mono or multilayer blown film, including biaxial oriented films, also for production of monofilament; can be used for injection molding and compounding.Tarn..
Tensile Modulus 0.100 GPa
14.5 ksi
1 mm/min
Arkema Group Evatane® 1003 VL 4C Ethylene Vinyl Acetate
EVA copolymer made by high pressure tubular process. Anti-UV stabilized grade. Applications Thermal and colorless agricultural film to 180 at 200 µ for greenhouse coverage.ISO data provided by the ..
Tensile Modulus 0.100 GPa
14.5 ksi
1 mm/min
Arkema Group Evatane® 1004 VL 4E Ethylene Vinyl Acetate
EVA copolymer made by high pressure tubular process. Anti-UV stabilized grade. Applications Thermal and colorless agricultural film to 180 at 200 µ for greenhouse coverage.ISO data provided by the ..
Tensile Modulus 0.100 GPa
14.5 ksi
1 mm/min
Arkema Group Evatane® 1020 VG 3 Ethylene Vinyl Acetate
EVA copolymer made by high process tubular process. Applications Grade for transparent films, high strength, sealing at low temperature, hot tack. Examples: laminates, coextrusion, secondary sealing..
Tensile Modulus 0.100 GPa
14.5 ksi
1 mm/min
Arkema Group Evatane® 1020 VN 3 Ethylene Vinyl Acetate
EVA copolymer made by high pressure tubular process. Applications Grade for flexible, very transparent films with high strength, very good sealability. Examples: thin stretch film for food packaging..
Tensile Modulus >= 0.100 GPa
>= 14.5 ksi
perpendicular to plane; ASTM C297
3A Composites Core Materials AIREX® T92.110 Easy Processing Structural Foam
AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,..