Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.00134 GPa | 0.195 ksi | ASTM D412 |
Aearo E-A-R Specialty Composites VersaDamp™ V-2325 TPE VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded.. |