Polymer Property : Tensile Modulus = 8.08 GPa
Polymer Property :
Tensile Modulus =
8.08 GPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Modulus
8.08
GPa
1170
ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP 2F006 ETFE