Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.54 GPa | 1090 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP ZFL24 PPE+PS LNP* LUBRICOMP* ZFL24 is a compound based on PPE+PS resin containing 20% Glass Fiber, 10% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Tensile Modulus | 7.54 GPa | 1090 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp ZFL24 PPO LNP* Lubricomp* ZFL24 is a compound based on Modified Polyphenylene Oxide (PPO) containing glass fiber and PTFE lubricant. Characteristics of this grade are: Internally Lubricated.This data was su.. |