Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.45 GPa | 1080 ksi | ASTM D638 |
Solvay Specialty Polymers Torlon® 4630 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4630 is an injection-moldable, wear-resistant grade of polyamide-imide (PAI), that has been formulated to give outstanding wear resistance in non-lubricated applications. Torlon PAI has the h.. |
|||
Tensile Modulus | 7.45 GPa | 1080 ksi | ASTM D638 |
Solvay Specialty Polymers Torlon® 4630 Polyamide-imide (PAI) Torlon® 4630 is an injection-moldable, wear-resistant grade of polyamide-imide (PAI), that has been formulated to give outstanding wear resistance in non-lubricated applications. Torlon® PAI h.. |
|||
Tensile Modulus | 7.45 GPa | 1080 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP 5E003M FP-V (PVDF) LNP* THERMOCOMP* 5E003M is a compound based on PVDF resin containing 15% Milled Carbon Fiber. Added feature of this grade is: Electrically Conductive. |