Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 60.0 GPa | 8700 ksi | ASTM D3039 |
Greene Tweed Orthetek® WF Polyketone, Continuous Woven Carbon Fiber Greene Tweed offers precision-molded thermoplastic components made from our high-performance Orthtek® composite materials for a variety of demanding medical and biotechnology applications. Ortht.. |
|||
Tensile Modulus | 60.0 GPa | 8700 ksi | |
Greene Tweed Xycomp® 1030-01 Carbon/Nylon 12 Composite Greene, Tweeds Xycomp® engineered components offer a wider range of benefits than conventional thermoset resin systems because they rely on thermoplastic resins for their matrix. With specific st.. |
|||
Tensile Modulus | 60.0 GPa | 8700 ksi | ASTM D3039 |
Greene Tweed WR™ 575 PEEK, Bi-Directional Carbon Fiber Filled WR®575 is a thermoplastic composite consisting of bi-directionally oriented carbon fibers in a PEEK matrix. The excellent wear resistance and the fiber orientation of WR575 makes this material i.. |
|||
Tensile Modulus | 60.0 - 90.0 GPa | 8700 - 13100 ksi | |
Goodfellow Nickel 55/Titanium 45 Shape Memory Alloy Shape memory alloy is a description applied to that group of metallic materials which show the ability to return to the previously defined shape or size when subjected to the correct thermal procedu.. |
|||
Tensile Modulus | 60.0 GPa @Temperature 135 °C |
8700 ksi @Temperature 275 °F |
90º, Wet; EN2561 |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 50%/G939 HS Carbon Information provided by HexCel |
|||
Tensile Modulus | 60.0 GPa @Temperature 75.0 °C |
8700 ksi @Temperature 167 °F |
90º, Wet; EN2561 |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 45% 46280 Fiber Information provided by HexCel |
|||
Tensile Modulus | 60.0 GPa @Temperature 23.0 °C |
8700 ksi @Temperature 73.4 °F |
0º, Conditioning: 23°C; ASTM D3039 |
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Woven Carbon Prepreg 42% resin weight with C193PW(HTA) - 193 g/m2 plain weave 3K HTA 49% fiber volumeInformation provided by HexCel |