Mechanical Properties Metric English Comments
Tensile Modulus 4.73 GPa
686 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP SH1100A PA12
LNP* Thermocomp* SH1100A is a Nylon 12, High Specificy Gravity compound containing proprietary fillers.
Tensile Modulus 4.73 GPa
686 ksi
Storage
Epoxy Technology EPO-TEK® EV2118-2 Silver-filled, electrically conductive epoxy
Preliminary Product Information SheetMaterial Description: A silver-filled, electrically conductive epoxy designed for semiconductor and electronic assembly.Information Provided by Epoxy Technology