Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.83 GPa | 555 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Cycolac® INP562 ABS SABIC INP562 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Tensile Modulus | 3.83 GPa | 555 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® INP562 ABS+SAN SABIC INP562 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Tensile Modulus | 3.83 GPa | 555 ksi | ISO 527-2/1A/1 |
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire PEEK is produced to the highest industry standards and is characteriz.. |
|||
Tensile Modulus | 3.83 GPa | 555 ksi | ISO 527-2/1A/1 |
Solvay Specialty Polymers KetaSpire® KT-820 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 NL is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire PEEK is produced to the highest industry standard.. |
|||
Tensile Modulus | 3.83 GPa | 555 ksi | 1 mm/min, Type 1A; ISO 527-2 |
Solvay Specialty Polymers KetaSpire® KT-820 NL Polyetheretherketone (PEEK) KetaSpire® KT-820 NL is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire® PEEK is produced to the highest industry .. |
|||
Tensile Modulus | 3.83 GPa | 555 ksi | 1 mm/min, Type 1A; ISO 527-2 |
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK) KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha.. |
|||
Tensile Modulus | 3.83 GPa | 555 ksi | 1 mm/min, Type 1A; ISO 527-2 |
Solvay Specialty Polymers KetaSpire® KT-XXXX Polyetheretherketone (PEEK) KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha.. |
|||
Tensile Modulus | 3.83 GPa | 556 ksi | ASTM D 638 |
Saint-Gobain Meldin® 3130 Thermoplastic Bearing Material Meldin 3130 components provide good strength and stiffness in addition to excellent high velocity performance. This formulation can be used with both hard or soft mating surfaces. Meldin® 3100 .. |
|||
Tensile Modulus | 3.83 GPa | 556 ksi | Storage |
Epoxy Technology EPO-TEK® E2116 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® E2116 is a two component, silver-filled and stencil printable electrically conductive adhesive for bonding SMDs onto PCB and substrates. Can be used as a “lead-free”.. |
|||
Tensile Modulus | 3.83 GPa | 556 ksi | 1 mm/min |
Arkema Group Rilsan® AZM 15 TLD Nylon 12, 15% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-030,GF15Rigid grade with glass fiber filler (15%) for injection molding.Available color: natural. Light and heat stabilized. Mold-release agent.Rigidity combined wi.. |