Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.86 GPa | 415 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Tensile Modulus | 2.86 GPa | 415 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Tensile Modulus | 2.86 GPa | 415 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Tensile Modulus | 2.86 GPa | 415 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® CX7720 PC+ABS (Asia Pacific) Cycoloy resin CX7720 is a non brominated and non chlorinated flame retardant PC/ABS resin grade featuring high heat resistance and thin wall FR. It is UL-94 listed at 1.2 mm V0 and 1.5mm 5VB. Its hi.. |
|||
Tensile Modulus | 2.86 GPa | 415 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Cycoloy® CY2000 PC+ABS Cycoloy resin CY2000 is a flame retardant (FR) PC/ABS blend free from halogen containing FR agents. It was designed to meet CA133 application requirements.This data was supplied by SABIC-IP for the .. |
|||
Tensile Modulus | 2.86 GPa | 415 ksi | ASTM D638 |
Quadrant EPP Acetron® MD Metal-detectable Copolymer Acetal (ASTM Product Data Sheet) Low moisture absorption High strength, stiffness Easy to machine No centerline porosity in Acetron® GP Many formulation options: Copolymer, Homopolymer, PTFE filled, and Internally lubricated/enha.. |
|||
Tensile Modulus | 2.86 GPa @Thickness 3.20 mm |
415 ksi @Thickness 0.126 in |
1mm/min; ASTM D638 |
LG Chemical GPPS 20HR(E) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
Tensile Modulus | 2.86 GPa | 415 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP KX06415 Acetal Copolymer LNP LUBRICOMP* KX06415 is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid Powder. Added features of this material include: Easy Molding, Heat Stabilized, Wear Resistant. |
|||
Tensile Modulus | 2.86 GPa | 415 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON KX96321 POM LNP* STAT-KON* KX96321 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Tensile Modulus | 2.86 GPa | 415 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL HN731A PPE+PS PPE+PS blend. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant (restrictions apply). Combine.. |
|||
Tensile Modulus | 2.86 GPa | 415 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP KAL22M Acetal Copolymer LNP LUBRICOMP* KAL22M is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant. |
|||
Tensile Modulus | 2.86 GPa | 415 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL 731 PPE+PS PPE+PS blend. Unfilled. NSF listed for potable water use in several colors (Standard 61). FDA compliant in several colors (restrictions apply). UL94 HB rated. Low water absorption. Hydrolytic stabi.. |
|||
Tensile Modulus | 2.86 GPa | 415 ksi | ASTM D790 |
Plastics Group Polifil® GFPC-10 10% Glass-Reinforced Polycarbonate Polifil® GFPC series compounds offer a combination of improved dimensional stability and decreased flammability. The excellent balance of physical properties make the Polifil® glass-filled polycar.. |
|||
Tensile Modulus | 2.86 - 2.90 GPa | 415 - 421 ksi | ASTM D638M |
DSM Somos® WaterClear® Ultra 10122 Optically Clear, Colorless, Rigid, Stereolithography Resin DescriptionDSM Somos® WaterClear Ultra 10122 is a next generation optically clear resin with ABS like properties and good temperature resistance. It produces colorless, functional, accurate parts .. |
|||
Tensile Modulus | 2.86 GPa | 415 ksi | 1 mm/min |
Arkema Group Nakan® RMS 501 L PVC, Rigid Injection Molding Grade NAKAN RMS 501 L is a rigid polyvinyl chloride compound developed for injection molding of electrical boxes ( inside ).ISO data provided by the manufacturer, Arkema. |
|||
Tensile Modulus | 2.86 GPa | 415 ksi | ASTM D-638 |
Axiall 7048A Rigid PVC, Extrusion Georgia Gulf 7048A is a general purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Impact Strength & ToughnessFlame RetardantColorabilityCert.. |
|||
Tensile Modulus | 2.86 GPa | 415 ksi | ASTM D-638 |
Axiall 9175 White 10 Rigid PVC, Molding, White 10 Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |