Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.322 GPa | 336.8 ksi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers ABSPC 7801 ABS/PC Injection Molding Grade, High Impact, High Heat Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Modulus | 2.322 GPa | 336.8 ksi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers ABSPC 7801E ABS/PC Extrusion Grade, High Impact, High Heat Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |