Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.21 GPa | 321 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EX1632T PC Lexan* EX1632T polycarbonate resin is designed for use in multi-wall sheet or profile extrusion applications. It contains branched polycarbonate resin, release, and UV stabilizer. It is available .. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1463T PC Copolymer (Asia Pacific) Lexan* EXL1463T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with medium flow ch.. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXE1413T PC Copolymer (Europe-Africa-Middle East) Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in "Energy" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color packa.. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® HPX4 PC Copolymer (Europe-Africa-Middle East) Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP.. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HPX4R PC Copolymer (Asia Pacific) Medium flow specialty polycarbonate with outstanding processability, ductility and autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatib.. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D638 |
Polymer Resources ABS-GP-HH General Purpose ABS, High Heat General Purpose Acrylonitrile Butadiene Styrene, High HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D638 |
Quadrant EPP Quadrant PC 1000 Extruded, Unfilled, Polycarbonate (ASTM Product Data Sheet) |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D882 |
Spartech PETG 3D Lenticular 3-D Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D638 |
Star Plastics ABS450FR Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | ASTM Data |
Styron CALIBRE™ MEGARAD 2080 15 Polycarbonate, Gamma Radiation Resistant CALIBRE® MegaRad 2080 series resins provide end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to high energy radiation (g.. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | ASTM Data |
Styron Magnum™ 541 ABS, High Impact MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D638 |
Westlake Plastics Absylux® FR Acrylonitrile-Butadiene-Styrene Flame Retardant Absylux ABS is a low cost engineering plastic that is easy to machine and fabricate. It is an ideal material for structural applications when impact resistance, strength, and stiffness are required.. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D638 |
Total PSI 830 Polystyrene Polystyrene 830 is a high melt flow, high impact polystyrene specially designed for hard to fill injection molding applications. The high flow 830 material aids production of stress free parts.The m.. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D-638 |
Axiall 8302 Rigid PVC, Extrusion & Molding Georgia Gulf 8302 is a clear rigid PVC pellet compound suited for applications where transparency is important in a high sunlight environment. It can be used for exterior transparent profiles such .. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D882 |
Spartech APET SP4110 Copolyester Sheet Description: Copolyester SheetInformation provided by Spartech. |
|||
Tensile Modulus | 2.21 GPa | 321 ksi | ASTM Data |
Styron Magnum™ 3490 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB.. |