Mechanical Properties Metric English Comments
Tensile Modulus 18.5 GPa
2680 ksi
ISO 527-1/-2
Lanxess Pocan® T 3150 XF 000000 PBT + PET, 55% Glass Fiber
PBT+PET, 55% glass fibers, injection molding, improved flowability, low tendency to warp, increased temperature peak load, increased strength and increased modulus
Tensile Modulus 18.5 GPa
2680 ksi
ISO 527-2
Solvay Specialty Polymers Kalix® 9950 Polyamide, High Performance (HPPA), 50% Glass Fiber
Kalix® 9950 is a 50% glass-fiber reinforced high-performance polyamide. It is hot-water moldable and intended for use in components requiring superior mechanical properties and excellent surface ..
Tensile Modulus 18.5 GPa
2680 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP EX93452 PEI
LNP THERMOCOMP* EX93452 is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Electrically Conductive.
Tensile Modulus 18.5 GPa
2680 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® LBV-65H FWA black 9225 PA12-GF65
Product description: Grilamid LBV-65H FWA black 9225 is a 65% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features High stiffness combined..
Tensile Modulus 18.5 GPa
2680 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® LBV-65H FWA nat PA12-GF65
Product description: Grilamid LBV-65H FWA natural is a 65% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w..
Tensile Modulus 18.5 GPa

@Temperature 23.0 °C
2680 ksi

@Temperature 73.4 °F
Akro-Plastic Akromid® T1 GF 50 (3101) PPA Dry, 50% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
Tensile Modulus 18.5 GPa
2680 ksi
1[mm/min]; ISO 527-1/2
Akro-Plastic Akromid® T1 GF 50 9 (3257) PPA Conditioned, 50% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..