Mechanical Properties Metric English Comments
Tensile Modulus 13.99 GPa
2029 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON EEF42 PEI
LNP STAT-KON* EEF42 is a compound based on Polyetherimide resin containing 10% Carbon Fiber, 20% Glass Fiber. Added features of this material include: Electrically Conductive.
Tensile Modulus 13.99 GPa
2029 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP VERTON RV008E PA 66
LNP* VERTON* RV008E is a compound based on Nylon 66 resin containing 40% Long Glass Fiber. Added features of this material include: Easy Molding, Structural.
Tensile Modulus 13.99 GPa
2029 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP VERTON RV008E PA 66 (Asia Pacific)
LNP* VERTON* RV008E is a compound based on Nylon 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding.
Tensile Modulus 13.99 GPa
2029 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON ME006 PP
LNP STAT-KON* ME006 is a compound based on Polypropylene resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.