Mechanical Properties Metric English Comments
Tensile Modulus 13.02 GPa
1888 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® CY-20GF/000 UV FR V0 PC/ABS Blend, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedIgnition ResistantNon-HalogenatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Modulus 13.02 GPa
1888 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP ZF0089 PPE+PS
LNP* THERMOCOMP* ZF0089 is a compound based on PPE+PS resin containing 40% Glass Fiber. Added features of this material include: Exceptional Processing, Flame Retardant.