Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.655 GPa | 240.0 ksi | |
Solvay Specialty Polymers Halar® 300 ECTFE Fluoropolymer
(discontinued **) Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing.. |
|||
Tensile Modulus | 1.655 GPa | 240.0 ksi | |
Solvay Specialty Polymers Halar® 500 ECTFE Fluoropolymer
(discontinued **) Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing.. |
|||
Tensile Modulus | 1.655 GPa | 240.0 ksi | ASTM D638 |
Ineos Styrenics Avantra® 2710 High Impact Styrenic Polymer (Global) Description: Avantra® 2710 is a high-impact grade of polystyrene with improved stress crack resistance, developed primarily for extrusion and thermoforming applications, especially for the refrig.. |
|||
Tensile Modulus | 1.655 GPa | 240.0 ksi | ASTM D638 |
Total PPH 3740WR Polypropylene, High Flow Nucleated Homopolymer Injection Molding Easy Flow TOTAL Polypropylene 3740WR exhibits exceptionally easy flow characteristics.FDA. 3740WR complies with all applicable FDA and USDA regulations and may be used under these provisions for .. |
|||
Tensile Modulus | 1.655 GPa | 240.0 ksi | ASTM D638 |
Total PPH 3860X Polypropylene Homopolymer, High Flow Reactor Grade for Non-Woven Fibers High Purity TOTAL Petrochemicals Polypropylene 3860X features extremely high purity for processing in micro denier fibers.Recommended Applications. 3860X is recommended for nonwoven fiber applicat.. |
|||
Tensile Modulus | 1.655 GPa @Temperature 45.0 °C |
240.0 ksi @Temperature 113 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S600F20 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provi.. |
|||
Tensile Modulus | 1.655 GPa @Temperature 45.0 °C |
240.0 ksi @Temperature 113 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S600F20UV WT660 Polybutylene Terephthalate (PBT) Unreinforced UV Stabilized Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provided.. |