Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.46 GPa | 212 ksi | ASTM Data |
Americas Styrenics Styron® 495R High Impact Polystyrene
(discontinued **) Data provided by Dow Chemical.Americas Styrenics was formed in 2008 as a joint venture between Dow Chemical and Chevron Phillips Chemical Company. Styron was a Dow trade name before the JV formatio.. |
|||
Tensile Modulus | 1.46 GPa | 212 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP TF002 PU LNP* THERMOCOMP* TF002 is a compound based on Polyurethane resin containing 10% Glass Fiber. |
|||
Tensile Modulus | 1.46 GPa | 212 ksi | ASTM D638 |
Azdel SuperLite® SL550600-100 PP Resin Matrix / 55% Glass Fiber (2.5 mm Molded Thickness) AZDEL SuperLite® SL550600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Tensile Modulus | 1.46 GPa | 212 ksi | 1mm/min |
Eastman Tenite 383A-12 CAP Cellulose Acetate Propionate
(discontinued **) 12% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |