Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.765 GPa | 111 ksi | 50 mm/min. Type I; ASTM D638 |
LyondellBasell Alathon® M5372 High Density Polyethylene ApplicationsALATHON M 5372 copolymer with narrow weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good processing stability. .. |
|||
Tensile Modulus | 0.765 GPa | 111 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® VB-5300GS PBT, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 0.765 GPa | 111 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® VB-5300GS PBT, Glass Filled FR Information provided by Samsung Cheil Industries. |