Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.276 GPa | 40.0 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Gravi-Tech™ GRV-UR-110-W Polyurethane, Unspecified (PUR, Unspecified) Information provided by PolyOne |
|||
Tensile Modulus | 0.276 - 0.345 GPa | 40.0 - 50.0 ksi | |
ITW Plexus Plexusâ„¢ MA425 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, long open time.Information provided by Illinois Tool Works. |
|||
Tensile Modulus | 0.276 - 0.345 GPa | 40.0 - 50.0 ksi | |
ITW Plexus Plexusâ„¢ MA556 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Standard for structural bonding in the marine industry.Information provided by Illinois Tool Works.. |
|||
Tensile Modulus | 0.276 - 0.345 GPa | 40.0 - 50.0 ksi | |
ITW Plexus Plexusâ„¢ MA550 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Excellent marine adhesive, UV stable.Information provided by Illinois Tool Works. |
|||
Tensile Modulus | 0.276 - 0.345 GPa | 40.0 - 50.0 ksi | |
ITW Plexus Plexusâ„¢ MA555 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low exotherm adhesive able to be used 1" thick.Information provided by Illinois Tool Works. |
|||
Tensile Modulus | 0.276 GPa | 40.0 ksi | ASTM D638 |
ScanTube MFA Tubing Information provided by ScanTube, Inc. |
|||
Tensile Modulus | 0.276 GPa | 40.0 ksi | ASTM D638 |
ScanTube PFA Tubing Information provided by ScanTube, Inc. |
|||
Tensile Modulus | 0.276 - 0.552 GPa | 40.0 - 80.0 ksi | |
Master Bond LED401 One Component LED Curable Adhesive System Master Bond LED401 is a highly innovative, one part LED type system that cures fully upon exposure to a 405 nm wavelength light source where the presence of any UV light is minimal or incidental. In.. |
|||
Tensile Modulus | 0.276 - 0.552 GPa | 40.0 - 80.0 ksi | |
Master Bond LED403Med USP Class VI, One Component, LED Curable System Master Bond LED403Med is a one part LED system that cures fully upon exposure to a 405 nm wavelength light that is generated by an LED source and. In fact, this material will fully cure tack-free wi.. |
|||
Tensile Modulus | 0.276 GPa | 40.0 ksi | 1 mm/min |
Arkema Group Pebax® 6333 SN 01 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) hardness 63 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: Sport (Football shoe sole, ski top lay.. |
|||
Tensile Modulus | 0.276 - 0.345 GPa | 40.0 - 50.0 ksi | |
ITW Plexus Plexus™ MA925 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, long open time.Information provided by Illinois Tool Works. |
|||
Tensile Modulus | 0.276 - 0.448 GPa | 40.0 - 65.0 ksi | ASTM D638 |
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Tensile Modulus | 0.276 GPa | 40.0 ksi | TM R050-36 |
Resinlab® EP1240RC Flame Retardant Epoxy Casting Resin Resinlab™ EP1240RC is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034, Pro.. |