Polymer Property : Tensile Modulus = 0.190 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.190 GPa

@Temperature 23.0 °C
27.6 ksi

@Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Hytrel® HTR8441 BK316 TPC-ET  (Unverified Data**)
Hytrel® HTR8441 is a 55 nom. Shore D thermoplastic polyester elastomer for blow molding. It provides good mechanical properties at high temperature.Information provided by DuPont Performance Polyme..
Tensile Modulus 0.190 GPa
27.6 ksi
ASTM D882
DuPont™ Sclairfilm® GL-1 LLDPE Film, Laminating, 38.1 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an..
Tensile Modulus 0.190 GPa
27.6 ksi
ASTM D882
DuPont™ Sclairfilm® GL-1 LLDPE Film, Laminating, 50.8 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an..
Tensile Modulus 0.190 GPa
27.6 ksi
ASTM D882
DuPont™ Sclairfilm® GL-1 LLDPE Film, Laminating, 76 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an..
Tensile Modulus 0.190 GPa
27.6 ksi
ASTM D882
DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 38.1 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an..
Tensile Modulus 0.190 GPa
27.6 ksi
ASTM D882
DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 50.8 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an..
Tensile Modulus 0.190 GPa
27.6 ksi
ASTM D882
DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 76 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an..
Tensile Modulus 0.190 GPa
27.6 ksi
LyondellBasell Lupolen® V 2520 J Ethylene Vinyl Acetate, Film Grade
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Tensile Modulus 0.190 GPa
27.6 ksi
MD/TD; ASTM D882-A
Borealis FA3220 Low Density Polyethylene
FA3220 is a Low Density Polyethylene for Film Extrusion. Autoclave Technology. Unmodified. This grade is developed to give a strong film with balanced shrink properties. Applications FA3220 has bee..
Tensile Modulus 0.190 GPa
27.6 ksi
MD/TD; ASTM D882-A
Borealis FA3227 Low Density Polyethylene
FA3227 is a Low Density Polyethylene for Film Extrusion. Autoclave Technology. Heat and U/V stabilized. This grade is suitable for building construction film and meets the requirements for heat, al..
Tensile Modulus 0.190 GPa
27.6 ksi
Bending Modulus; ASTM D790
UBE UMERIT 1500F Metallocene LLDPE
Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical propert..
Tensile Modulus 0.190 GPa
27.6 ksi
Bending Modulus; ASTM D790
UBE UMERIT 1520F Metallocene LLDPE
Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical propert..
Tensile Modulus >= 0.190 GPa
>= 27.6 ksi
perpendicular to plane; ASTM C297
3A Composites Core Materials AIREX® T92.200 Easy Processing Structural Foam
AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable, UV r..