Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.100 GPa | 14.5 ksi | 1mm/min; DIN 53457 |
Advanced Elastomer Systems VistaFlex® 715-N Thermoplastic Rubber
(discontinued **) Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f.. |
|||
Tensile Modulus | 0.100 GPa @Temperature 23.0 °C |
14.5 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® HTR8685 BK022A TPC-ET
(Unverified Data**) Hytrel® HTR8685 BK022A is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal hardness of 44D, is pigmented black with fine particle size carbon black,.. |
|||
Tensile Modulus | 0.100 GPa | 14.5 ksi | |
LATI Latigray 47/1-01 CX/45 PP Copolymer Radiopaque compound based on Polypropylene copolymer (PPc). Special mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati .. |
|||
Tensile Modulus | 0.100 - 0.300 GPa @Thickness 2.00 mm |
14.5 - 43.5 ksi @Thickness 0.0787 in |
1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 32008 Polyvinylidene Fluoride (PVDF) Solef® 32008 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional .. |
|||
Tensile Modulus | 0.100 GPa | 14.5 ksi | ISO 527-1/-2 |
DSM Arnitel® EM460 46 Shore D, Injection Molding or Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.100 GPa | 14.5 ksi | ISO 527-1/-2 |
DSM Arnitel® EM460 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.100 GPa | 14.5 ksi | ISO 527-1/-2 |
DSM Arnitel® PL420-H Injection Molding Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.100 GPa | 14.5 ksi | ISO 527-1/-2 |
DSM Arnitel® PL420-H Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.100 GPa | 14.5 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® HTR8685 BK022A Polyester Elastomer TPC-ET
(Unverified Data**) 44 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Hytrel HTR8685 BK022A is designed for blow molding or processing techniques requi.. |
|||
Tensile Modulus | 0.100 GPa | 14.5 ksi | cond.; ISO 527 |
Azoty Tarnow™ Tarnamid® T-29 MS Polyamide 6 - Natural Medium-high viscosity extrusion grade for mono or multilayer blown film, including biaxial oriented films, also for production of monofilament; can be used for injection molding and compounding.For .. |
|||
Tensile Modulus | 0.100 GPa | 14.5 ksi | cond.; ISO 527 |
Azoty Tarnow™ Tarnamid® T-29 Polyamide 6 - Natural Medium-high viscosity extrusion grade for mono or multilayer blown film, including biaxial oriented films, also for production of monofilament; can be used for injection molding and compounding.Tarn.. |
|||
Tensile Modulus | 0.100 GPa | 14.5 ksi | 1 mm/min |
Arkema Group Evatane® 1003 VL 4C Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Anti-UV stabilized grade. Applications Thermal and colorless agricultural film to 180 at 200 µ for greenhouse coverage.ISO data provided by the .. |
|||
Tensile Modulus | 0.100 GPa | 14.5 ksi | 1 mm/min |
Arkema Group Evatane® 1004 VL 4E Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Anti-UV stabilized grade. Applications Thermal and colorless agricultural film to 180 at 200 µ for greenhouse coverage.ISO data provided by the .. |
|||
Tensile Modulus | 0.100 GPa | 14.5 ksi | 1 mm/min |
Arkema Group Evatane® 1020 VG 3 Ethylene Vinyl Acetate EVA copolymer made by high process tubular process. Applications Grade for transparent films, high strength, sealing at low temperature, hot tack. Examples: laminates, coextrusion, secondary sealing.. |
|||
Tensile Modulus | 0.100 GPa | 14.5 ksi | 1 mm/min |
Arkema Group Evatane® 1020 VN 3 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for flexible, very transparent films with high strength, very good sealability. Examples: thin stretch film for food packaging.. |
|||
Tensile Modulus | >= 0.100 GPa | >= 14.5 ksi | perpendicular to plane; ASTM C297 |
3A Composites Core Materials AIREX® T92.110 Easy Processing Structural Foam AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,.. |