Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.0138 GPa | 2.00 ksi | TM R050-36 |
Resinlab® EP1121 Clear Electronic Grade Epoxy Encapsulant Resinlab™ EP1121 Clear is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexible polymer. I.. |
|||
Tensile Modulus | 0.0138 GPa | 2.00 ksi | 500%; ASTM D412/D638 |
Lubrizol Estane® MVT 80AF3 Thermoplastic Polyurethane, Moisture Vapor Transmission Type: Estane® MVT 80AF3 TPU is a aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission, good low temperature properties and elasticity.Uses: Blown and.. |
|||
Tensile Modulus | 0.0138 GPa @Thickness 0.127 mm |
2.00 ksi @Thickness 0.00500 in |
Cured; ASTM D638 |
Aptek DAT-A-THERM 1000 Electrically insulating urethane film DAT-A-THERM 1000 is a tough, flexible, void free, electrically insulating urethane film designed to fill air gaps and dissipate heat between devices and substrates. DAT-A-THERM 1000 film is a 100% s.. |
|||
Tensile Modulus | 0.0138 GPa | 2.00 ksi | Molded Properties; ASTM D638 |
ExxonMobil Escorene™ AD 2528EH2 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: AD 2528EH2 is a copolymer of ethylene and vinyl acetate. Availability: Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: YesFree Flowing Agent: Yes Applications:Hot Mel.. |
|||
Tensile Modulus | 0.0138 GPa | 2.00 ksi | ASTM D1708 |
DuPont Elvax® 4355 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 4355 is an ethylene-vinyl acetate / acid terpolymer resin for use in industrial applications.ApplicationsElvax® 4355 resins can be used for the following applications: adhesives, s.. |
|||
Tensile Modulus | 0.0138 GPa | 2.00 ksi | TM R050-36 |
Resinlab® EP1121 Black Electronic Grade Epoxy Encapsulant Resinlab™ EP1121 Black is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexible polymer. I.. |