Polymer Property : Hydrostatic Design Basis = 11.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Hydrostatic Design Basis 11.0 MPa

@Temperature 22.8 °C
1600 psi

@Temperature 73.0 °F
ASTM D2837
Total HDPE XT10 N High Density Polyethylene - Pipe Resin
Polyethylene: High molecular weight, bimodal pipe resin.Characteristics:Outstanding high temperature creep rupture strengthExceptional slow crack growth resistanceExcellent resistance to rapid crac..
Hydrostatic Design Basis 11.0 MPa

@Temperature 22.8 °C
1600 psi

@Temperature 73.0 °F
ASTM D2837
Total HDPE XT10B High Density Polyethylene, Pipe Resin
Polyethylene: HDPE Bimodal PE4710 pipe resin (Black)Characteristics:Outstanding high temperature creep rupture strengthOutstanding slow crack growth resistanceExcellent resistance to rapid crack pr..
Hydrostatic Design Basis 11.0 MPa

@Temperature 22.8 °C
1600 psi

@Temperature 73.0 °F
ASTM D2837
Total HDPE XT25N High Density Polyethylene, Pipe Resin
Polyethylene: High molecular weight, bimodal pipe resin. PPI TR4 designation PE4710 /PE100 for demanding installations. Every batch certified to meet 2500 hrs PENT according to ASTM F1473.Charact..
Hydrostatic Design Basis 11.0 MPa

@Temperature 23.0 °C
1600 psi

@Temperature 73.4 °F
ASTM D2837
Chevron Phillips Marlex® H516HP High Density Polyethylene, Pressure Pipe Grade
This high performance PE 4710 HDPE is tailored for the demands of pressure pipe applications that require:Excellent long-term hoop strengthSuperb resistance to slow crack growthExceptional resistanc..
Hydrostatic Design Basis 11.0 MPa

@Temperature 23.0 °C
1600 psi

@Temperature 73.4 °F
ASTM D2837
Chevron Phillips Marlex® H525 High Density Polyethylene, Pressure Pipe Grade
This high performance PE 4710 HDPE is tailored for demanding pressure pipe applications that require:Good long-term hoop strengthGood resistance to slow crack growthExcellent resistance to slumpAddi..
Hydrostatic Design Basis 11.0 MPa

@Temperature 23.0 °C
1600 psi

@Temperature 73.4 °F
ASTM D2837
Chevron Phillips Marlex® HP132 High Density Polyethylene, Pressure Pipe Grade
This high performance PE 4710 HDPE is tailored for the demands of pressure pipe applications that require:Excellent long-term hoop strengthSuperb resistance to slow crack growthExceptional resistanc..