Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 5.17 MPa | 750 psi | at 100%; ASTM D412 |
5187 Polyurethane-based Biomedical Elastomer |
|||
Tensile Strength, Yield | 5.17 MPa | 750 psi | ASTM D638 |
Multibase Multi-Flex® G 7155 TPE Styrene Ethylene Butylene Styrene Block Copolymer Features: Chemical Resistance, Good Noise DampingOzone Resistant Thermal Stability, Good Forms:PelletsProcessing Method:Injection MoldingBlow MoldingExtrusion Uses: Automotive ApplicationsInforma.. |
|||
Tensile Strength, Yield | 5.17 MPa | 750 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® A 4710 S Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Method:Injection Molding Information provided by Multibase |
|||
Tensile Strength, Yield | 5.17 MPa | 750 psi | Tensile strength decreases by 10% after dry heat aging for 70 hrs at 437°F.; ASTM D412 |
Saint-Gobain COHRlastic® 9070 Wide Series General Purpose Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Tensile Strength, Yield | 5.17 MPa | 750 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3300-70 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Food Service Applications, Medical Applications, TubingAppearance-ClearForms-PelletsProcessing-Extrusio.. |
|||
Tensile Strength, Yield | 5.17 MPa | 750 psi | ASTM D412 |
Teknor Apex UNIPRENE® 7100-64 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 5.17 MPa | 750 psi | |
Master Bond Mastersil 702 One Component, Room Temperature Curing Silicone Elastomer Master Bond Master Sil 702 is ready-to-use, one component high performance silicone elastomer compound for bonding and sealing. Master Sil 702 is heat resistant to 450°F. It is supplied as an easy .. |
|||
Tensile Strength, Yield | >= 5.17 MPa @Temperature 204 °C |
>= 750 psi @Temperature 400 °F |
Flatwise Tensile; After 500 hrs at 400°F (Weight loss = 0.75%); Composite Honeycomb Sandwich Performance; ASTM C 297 |
Hexcel® Redux® HP655 Toughened BMI film Adhesive Redux® HP655 is a toughened BMI structural adhesive designed for metal to metal, composite to composite, and honeycomb sandwich bonding for both co-cured and precured composite skins. Redux® HP655.. |
|||
Tensile Strength, Yield | 5.17 MPa @Strain 100 % |
750 psi @Strain 100 % |
ASTM D412 |
Clariant OMAN698583 Thermoplastic Polyurethane, Halogen Free, Flame Retardant Aromatic Polyether BasedData provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 5.17 MPa | 750 psi | ASTM D412 |
Elastocon TPE Technologies Elastocon® STK56PA Thermoplastic Elastomer Elastocon® STK56PA thermoplastic elastomer has been developed for applications that require soft rubber-like properties and a good surface finish. Elastocon® STK56PA is well suited for consumer go.. |
|||
Tensile Strength, Yield | 5.17 MPa | 750 psi | ASTM D638 |
Dow AMPLIFY™ VA 400 Ethylene vinyl acetate (EVA) AMPLIFY™ VA 400 Functional Polymer is produced via a high pressure reactor. It exhibits high flexibility, clarity and low temperature sealability. It is easy to process and features functional .. |
|||
Tensile Strength, Yield | 5.17 MPa | 750 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® IT 37-023 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledApplications:General PurposeMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingPolyOne First ChoiceInformation .. |
|||
Tensile Strength, Yield | 5.17 MPa | 750 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3302-65 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses- Medical Applications, Tubing, Appearance-ClearForms-PelletsProcessing-ExtrusionInformation provided by.. |
|||
Tensile Strength, Yield | 5.17 MPa @Strain 300 % |
750 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® IT 37-031 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Specialty Thermoplastic ElastomerMarket:IndustrialConsumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation. |