Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 260 - 470 MPa @Strain 0.200 % |
37700 - 68200 psi @Strain 0.200 % |
|
ALIMEX PLANAL 7075 T651/T652 Aluminum Alloy Aluminium rolled plates which have been machined on both sides. Has a precise surface finish and high tensile strength. The temper values and the material conditions are not changed by surface-machi.. |
|||
Tensile Strength, Yield | 260 - 470 MPa @Strain 0.200 % |
37700 - 68200 psi @Strain 0.200 % |
|
ALIMEX 7075 T651/T652 Aluminum Alloy Rolled Rolled aluminium material according to DIN EN standard. Information provided by ALIMEX GmbHSolution heat treated, stress-relieved by stretching a controlled amount then artificially aged. / Solution.. |