Mechanical Properties Metric English Comments
Tensile Strength, Yield 276 - 345 MPa

@Strain 0.200 %
40000 - 50000 psi

@Strain 0.200 %
Materion BrushCAST® 20C High Strength Casting Alloy (As Cast)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Tensile Strength, Yield 276 - 345 MPa

@Strain 0.200 %
40000 - 50000 psi

@Strain 0.200 %
Materion BrushCAST® 21C High Strength Casting Alloy (As Cast)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Tensile Strength, Yield 170 - 345 MPa
24700 - 50000 psi
Materion Brush 1915â„¢ AT Temper Rod
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe..
Tensile Strength, Yield 276 - 345 MPa

@Strain 0.200 %
40000 - 50000 psi

@Strain 0.200 %
Materion BrushCAST® 20CT Fine Grain Casting Alloy (As Cast)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Tensile Strength, Yield 207 - 345 MPa

@Strain 0.200 %
30000 - 50000 psi

@Strain 0.200 %
Annealed temper
Special Metals INCONEL® 601GC® Nickel Superalloy
Data provided by the manufacturer, Special Metals.
Tensile Strength, Yield 283 - 345 MPa
41000 - 50000 psi
0.2% offset
Eagle Brass 110 EPT COPPER, Hard
Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of ..
Tensile Strength, Yield 276 - 345 MPa
40000 - 50000 psi
0.2% offset
Eagle Brass 151 ZHC® COPPER, 1/2 Hard
Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c..
Tensile Strength, Yield 241 - 345 MPa
35000 - 50000 psi
0.2% offset
Eagle Brass 240 Low Brass, 1/2 Hard
CDA 240 has excellent ductility, corrosion resistance and strength which allows it to be deep drawn, etched, stamped, blanked and bent. Typical uses include musical instruments, battery caps, flexib..
Tensile Strength, Yield 138 - 345 MPa
20000 - 50000 psi
0.2% offset
Eagle Brass 511 Phosphor Bronzes 4%, 1/4 Hard
511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge..
Tensile Strength, Yield 103 - 345 MPa
15000 - 50000 psi
Chicago Extruded Metals UNS C34500 Copper-Zinc-Lead Alloy
Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available in rods.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals
Tensile Strength, Yield 283 - 345 MPa
41000 - 50000 psi
0.2% offset
Eagle Brass 101 OFE COPPER (Certified), Hard
Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information..
Tensile Strength, Yield 283 - 345 MPa
41000 - 50000 psi
0.2% offset
Eagle Brass 102 OF COPPER (Non-Certified), Hard
Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an..
Tensile Strength, Yield 317 - 345 MPa
46000 - 50000 psi
Chicago Extruded Metals BioBrass® CXM10 Lead-Free Alloy
Finished product available in rods.Chicago Extruded Metal temper code: H02This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metals
Tensile Strength, Yield 276 - 345 MPa

@Strain 0.200 %
40000 - 50000 psi

@Strain 0.200 %
AK Steel 436L ULTRA FORM® Ferritic Stainless Steel
AK Steel’s 436L ULTRA FORM® is a ferritic grade of stainless steel that outperforms Type 409 in oxidation resistance and corrosion testing. The addition of molybdenum enhances pitting resistance w..