Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 14.0 - 21.0 MPa | 2030 - 3050 psi | ASTM D638 |
Arkema Group KYNAR FLEX® 2950-05 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toug.. |
|||
Tensile Strength, Yield | 3.10 - 21.0 MPa | 450 - 3050 psi | Average value: 14.0 MPa Grade Count:25 |
Overview of materials for Ionomer, Molded This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Tensile Strength, Yield | 8.30 - 21.0 MPa | 1200 - 3050 psi | Average value: 11.5 MPa Grade Count:59 |
Overview of materials for Low Density Polyethylene (LDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi.. |
|||
Tensile Strength, Yield | 14.0 - 21.0 MPa | 2030 - 3050 psi | ASTM D638 |
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |