Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 158 - 188 MPa | 22900 - 27300 psi | Average value: 168 MPa Grade Count:4 |
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m.. |