Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 500 - 750 MPa @Strain 0.200 % |
72500 - 109000 psi @Strain 0.200 % |
|
SSAB Tunnplat Docol® 1000 DL High-strength Steel In course of development.Data provided by SSAB Tunnplat. |
|||
Tensile Strength, Yield | 550 - 750 MPa @Strain 0.200 % |
79800 - 109000 psi @Strain 0.200 % |
|
CLAL-MSX DECLAFOR® 1015 TH1 Rod quenched/Cold Rolled/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Tensile Strength, Yield | 600 - 750 MPa | 87000 - 109000 psi | |
ArcelorMittal Dual Phase 980 LCE Y600 Very high strength steel, Cold Rolled Steel Available in the following: HCT980X (uncoated), HCT980X+ZE (electrogalvanized) and HCT980X+Z/ZF (Extragal®/Galvannealed)Description: Dual Phase steels offer an outstanding combination of strength a.. |
|||
Tensile Strength, Yield | 620 - 750 MPa | 89900 - 109000 psi | |
ArcelorMittal Complex Phase Steel 750 Very high strength steel, Hot Rolled Steel Available in the following: uncoated (HCT750C) and Extragal®/Galvannealed (HCT750C+Z)Description: The Complex Phase family of steels supplements ArcelorMittal's VHSS (very high strength steel) prod.. |