Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 62.7 MPa | 9090 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding M4825 Polyvinyl Chloride, Rigid (PVC, Rigid) ** NOTE: UL REGULATORY LISTING PENDINGInformation provided by PolyOne |