Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 0.621 MPa | 90.0 psi | ASTM D412 |
Saint-Gobain COHRlastic® R10470 Medium General-Purpose Silicone Sponge Rubber Description: Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six cons.. |
|||
Tensile Strength, Yield | 0.621 MPa | 90.0 psi | ASTM D412 |
Saint-Gobain COHRlastic® 100S Silicone Sponge/High Temp Silicone Adhesive Pressure Sensitive Tape Description: Strip-N-Stick® tape provides all the benefits of silicone rubber in an easy-to-apply, pressure-sensitive adhesive tape form. Compressible and flexible, it can conform to irregular su.. |
|||
Tensile Strength, Yield | 0.621 MPa @Strain 300 % |
90.0 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® RT-3820M Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerTransparentApplications:FDA (Food Contact)Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingDisclaimer: A thermoplasti.. |
|||
Tensile Strength, Yield | 0.621 MPa @Strain 300 % |
90.0 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® ST-6120 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerTransparentOver-Molding GradeApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne .. |