Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 57.23 MPa | 8301 psi | 2 in per min; ASTM D638 |
Network Polymers MS 200 Styrene Methyl Methacrylate Copolymer Description: Styrene Methyl Methacrylate CopolymerInformation provided by Network Polymers Inc. |