Mechanical Properties Metric English Comments
Tensile Strength, Yield 5.17 MPa
750 psi
at 100%; ASTM D412
5187 Polyurethane-based Biomedical Elastomer
Tensile Strength, Yield 5.17 MPa
750 psi
ASTM D638
Multibase Multi-Flex® G 7155 TPE Styrene Ethylene Butylene Styrene Block Copolymer
Features: Chemical Resistance, Good Noise DampingOzone Resistant Thermal Stability, Good Forms:PelletsProcessing Method:Injection MoldingBlow MoldingExtrusion Uses: Automotive ApplicationsInforma..
Tensile Strength, Yield 5.17 MPa
750 psi
Elastic; ASTM D412
Multibase Multi-Flex® A 4710 S Black TPE Thermoplastic Elastomer
Forms: PelletsProcessing Method:Injection Molding Information provided by Multibase
Tensile Strength, Yield 5.17 MPa
750 psi
Tensile strength decreases by 10% after dry heat aging for 70 hrs at 437°F.; ASTM D412
Saint-Gobain COHRlastic® 9070 Wide Series General Purpose Silicone Solid Rubber
Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome..
Tensile Strength, Yield 5.17 MPa
750 psi
100%; ASTM D412
Teknor Apex APEX® 3300-70 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Food Service Applications, Medical Applications, TubingAppearance-ClearForms-PelletsProcessing-Extrusio..
Tensile Strength, Yield 5.17 MPa
750 psi
ASTM D412
Teknor Apex UNIPRENE® 7100-64 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tensile Strength, Yield 5.17 MPa
750 psi
Master Bond Mastersil 702 One Component, Room Temperature Curing Silicone Elastomer
Master Bond Master Sil 702 is ready-to-use, one component high performance silicone elastomer compound for bonding and sealing. Master Sil 702 is heat resistant to 450°F. It is supplied as an easy ..
Tensile Strength, Yield >= 5.17 MPa

@Temperature 204 °C
>= 750 psi

@Temperature 400 °F
Flatwise Tensile; After 500 hrs at 400°F (Weight loss = 0.75%); Composite Honeycomb Sandwich Performance; ASTM C 297
Hexcel® Redux® HP655 Toughened BMI film Adhesive
Redux® HP655 is a toughened BMI structural adhesive designed for metal to metal, composite to composite, and honeycomb sandwich bonding for both co-cured and precured composite skins. Redux® HP655..
Tensile Strength, Yield 5.17 MPa

@Strain 100 %
750 psi

@Strain 100 %
ASTM D412
Clariant OMAN698583 Thermoplastic Polyurethane, Halogen Free, Flame Retardant
Aromatic Polyether BasedData provided by Clariant Masterbatches
Tensile Strength, Yield 5.17 MPa
750 psi
ASTM D412
Elastocon TPE Technologies Elastocon® STK56PA Thermoplastic Elastomer
Elastocon® STK56PA thermoplastic elastomer has been developed for applications that require soft rubber-like properties and a good surface finish. Elastocon® STK56PA is well suited for consumer go..
Tensile Strength, Yield 5.17 MPa
750 psi
ASTM D638
Dow AMPLIFY™ VA 400 Ethylene vinyl acetate (EVA)
AMPLIFY™ VA 400 Functional Polymer is produced via a high pressure reactor. It exhibits high flexibility, clarity and low temperature sealability. It is easy to process and features functional ..
Tensile Strength, Yield 5.17 MPa
750 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
PolyOne Synprene® IT 37-023 Thermoplastic Elastomer - SBC, Mineral Filled  (discontinued **)
Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledApplications:General PurposeMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingPolyOne First ChoiceInformation ..
Tensile Strength, Yield 5.17 MPa
750 psi
100%; ASTM D412
Teknor Apex APEX® 3302-65 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses- Medical Applications, Tubing, Appearance-ClearForms-PelletsProcessing-ExtrusionInformation provided by..
Tensile Strength, Yield 5.17 MPa

@Strain 300 %
750 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
PolyOne Synprene® IT 37-031 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:Specialty Thermoplastic ElastomerMarket:IndustrialConsumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation.