Polymer Property : Tensile Strength, Yield = 692 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 4.77 MPa
>= 692 psi
Stress at Elongation M50; ASTM D412 Method A
Seals Eastern 7182E Fluorocarbon-Elastomer
Formulated AFLAS® high-temperature "sour" oil & gas service. Excellent acid and base resistance.Information provided by Seals Eastern, Inc.