Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 465 MPa @Strain 0.200 % |
67400 psi @Strain 0.200 % |
|
Haynes 188 alloy, cold rolled and 1175°C solution annealed sheet Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Tensile Strength, Yield | 465 MPa @Strain 0.200 % |
67400 psi @Strain 0.200 % |
|
Haynes 556® alloy, all-weld metal GTAW Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |