Mechanical Properties Metric English Comments
Tensile Strength, Yield 462 MPa

@Strain 0.200 %
67000 psi

@Strain 0.200 %
Haynes Hastelloy® G-30® alloy, all-weld metal, GMAW weld 1.1 mm diameter filler wire
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Tensile Strength, Yield 462 MPa

@Strain 0.200 %
67000 psi

@Strain 0.200 %
Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed + 10% Cold Work
Tensile strength (ultimate and yield), elongation, and reduction of area values are for annealed then cold worked samples. This produces ASTM grain size 9.0. Other property values are typical of t..
Tensile Strength, Yield 462 - 510 MPa
67000 - 74000 psi
0.2% offset
Eagle Brass 194 HSM® Copper, Spring
High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and pl..
Tensile Strength, Yield 462 - 510 MPa
67000 - 74000 psi
0.2% offset
Eagle Brass 220 Commercial Bronze, Extra Spring
CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum..
Tensile Strength, Yield 462 - 538 MPa
67000 - 78000 psi
0.2% offset
Eagle Brass 260 Cartridge Brass, Hard
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
Tensile Strength, Yield 462 - 552 MPa
67000 - 80000 psi
0.2% offset
Eagle Brass 425 Tin Brass 2%, Hard
Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector..
Tensile Strength, Yield 462 - 572 MPa
67000 - 83000 psi
0.2% offset
Eagle Brass 519 Phosphor Bronzes 6%, 3/4 Hard
Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C..
Tensile Strength, Yield 462 - 538 MPa
67000 - 78000 psi
0.2% offset
Eagle Brass 735 Nickel Silver 18%, Hard
735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company
Tensile Strength, Yield 462 MPa

@Strain 0.200 %,
Temperature -129 °C
67000 psi

@Strain 0.200 %,
Temperature -200 °F
Transverse
Carpenter 20Cb-3® Stainless Steel
Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re..
Tensile Strength, Yield 462 MPa

@Strain 0.200 %,
Temperature 566 °C
67000 psi

@Strain 0.200 %,
Temperature 1050 °F
Carpenter Custom 450® Stainless Steel, Condition H1150 (Age Hardened 621°C)
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..
Tensile Strength, Yield 462 MPa

@Strain 0.200 %
67000 psi

@Strain 0.200 %
Haynes Hastelloy® C-22® alloy, transverse, GTAW spray weldment, 12.7 mm (1/2 in.) thick plate
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al..