Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 4.52 MPa | 655 psi | AVG Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 5484 Nitrile Rubber Low temperature service NitrileInformation provided by Seals Eastern, Inc. |