Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 4.31 MPa | 625 psi | 200%, post cured- 4 hours at 204°C |
Multibase SILASTIC® C7-4565 TBPB Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 4.31 MPa | 625 psi | ASTM D412 |
Polymax® Maxelast® C4630 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Tensile Strength, Yield | 4.31 MPa | 625 psi | @50% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® 571 Perfluoroelastomer Chemraz® 571 is recommended for a wide variety of semiconductor equipment wet processing applications where stringent seal reliability and contamination control are required. This seal material .. |
|||
Tensile Strength, Yield | 4.31 MPa | 625 psi | @50% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® 585 Perfluoroelastomer Chemraz® 585, a perfluoroelastomer, is a specialty cream compound formulated to outlast the most demanding chemical process applications. With its outstanding overall chemical resistance, Chemra.. |
|||
Tensile Strength, Yield | 4.31 MPa | 625 psi | @50% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® SD585 Perfluoroelastomer Chemraz® SD 585, a cream-colored perfluoroelastomer, offers the broadest chemical resistance of any elastomer, combining the resilience and sealing force of an elastomer with chemical resistance .. |
|||
Tensile Strength, Yield | 4.31 MPa | 625 psi | @50% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® 639 Perfluoroelastomer Chemraz® 639 perfluoroelastomer is specifically developed by Greene Tweed to meet the rigorous demands of aggressive plasma systems. This product’s unique formulation provides enhanced plas.. |
|||
Tensile Strength, Yield | 4.31 MPa | 625 psi | ASTM D412 |
Teknor Apex Vidux® CV-1000-76 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-AntistaticForms-PelletsProcessing Method- ExtrusionInformation provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 4.31 MPa | 625 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® IT 454 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerApplications:General PurposeCove BaseInteriorMarket:AutomotiveConsumer GoodsBuilding and ConstructionProcessing Method:Extrusion and Molding.. |