Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 41.9 MPa @Thickness 3.20 mm |
6070 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUCEL HI515W POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: Gears, Automobile ClipCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical |