Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 415 MPa | >= 60200 psi | |
MetalTek C86300 High Tensile Manganese Bronze High strength and hardness copper-zinc alloy.Applications: Steel mill nuts, ordnance parts, worm gears.Information provided by MetalTekCast UNS C86300; Cast Grade C86300; Cast ASTM B271, B584, B148;.. |
|||
Tensile Strength, Yield | >= 415 MPa | >= 60200 psi | |
MetalTek MTEK 220-01 Cast UNS J82090 Martensitic Stainless Steel Information provided by MetalTek |
|||
Tensile Strength, Yield | >= 415 MPa | >= 60200 psi | |
MetalTek MTEK 2205 Cast UNS J92205 Duplex Stainless Steel Excellent seawater corrosion resistance combined with nearly twice the strength of common stainless steels.Applications: Offshore piping systems, couplings. Centrifuge, dewatering equipment. Pump, v.. |
|||
Tensile Strength, Yield | >= 415 MPa | >= 60200 psi | |
MetalTek MTEK 221-01 Cast UNS J84090 Martensitic Stainless Steel Information provided by MetalTek |
|||
Tensile Strength, Yield | >= 415 MPa | >= 60200 psi | |
MetalTek MTEK 222-01 Cast UNS J82090 Martensitic Stainless Steel Information provided by MetalTek |
|||
Tensile Strength, Yield | >= 415 MPa | >= 60200 psi | |
MetalTek MTEK 223-01 Cast UNS J84090 Martensitic Stainless Steel Information provided by MetalTek |
|||
Tensile Strength, Yield | >= 415 MPa | >= 60200 psi | |
MetalTek MTEK 230-B Cast UNS C95500HT Aluminum Bronze Versatile alloy with high strength, good ductility, unusual toughness, plus exceptional wear resistance. Aluminum Bronze heat treated to higher mechanical properties where necessary.Information prov.. |
|||
Tensile Strength, Yield | >= 415 MPa | >= 60200 psi | |
MetalTek MTEK B Cast UNS N24030 Nickel-Copper Alloy Family of alloys for extreme heat and corrosion services.Applications: Gas Turbine parts. Chemical process equipment, heat treating equipment.Information provided by MetalTek |
|||
Tensile Strength, Yield | 415 MPa | 60200 psi | |
Haynes Hastelloy® W alloy as a weld filler, base metal Carbon steel 12.7 mm plate weldments Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Tensile Strength, Yield | 415 MPa @Strain 0.200 %, Temperature 870 °C |
60200 psi @Strain 0.200 %, Temperature 1600 °F |
|
Haynes Waspaloy™ alloy, sheet Age-hardenable superalloy with very good strength at temperatures up 980°C (1800°F), can be cold-formed in the annealed condition, may also be hot formed at 1040°C (1900°F) and above, go.. |
|||
Tensile Strength, Yield | 415 MPa @Temperature 22.0 °C |
60200 psi @Temperature 71.6 °F |
25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® HPC 1300 Unsaturated Polyester UP HPC 1300 is a special SMC for high strength applications. The glass level has been selected to combine mouldability with high strength and stiffness properties in orientation direction. The reinforc.. |
|||
Tensile Strength, Yield | 415 MPa @Strain 0.200 % |
60200 psi @Strain 0.200 % |
|
Haynes 25 alloy, vacuum investment castings, solution treated Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Tensile Strength, Yield | 415 MPa | 60200 psi | Annealed |
Special Metals INCONEL® Alloy C-276 A nickel-molybdenum-chromium alloy with an addition of tungsten having excellent corrosion resistance in a wide range of severe environments. The high molybdenum content makes the alloy especially .. |
|||
Tensile Strength, Yield | 415 MPa | 60200 psi | 90º, RT, Dry; EN2561 |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 37%/7781 Fiber Information provided by HexCel |
|||
Tensile Strength, Yield | 415 MPa @Strain 0.200 % |
60200 psi @Strain 0.200 % |
|
CRP Technology 8601 Aerospace Grade Power Metallurgy Aluminum Alloy For Motorsport and Aerospace marketplaces: manufactured by a special powder metallurgy process using a high-energy mixing process which ensures excellent mechanical properties.Super Aluminium materi.. |
|||
Tensile Strength, Yield | 415 MPa @Strain 0.200 % |
60200 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum E-BRITE 26-1® Superferritic Stainless Steel, UNS S44627 Property data below is typical of annealed samples. High purity superferritic stainless steel. Available in sheet and strip for use in chemical process equipment to combat chloride pitting and stre.. |