Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 353 MPa @Strain 0.200 % |
51200 psi @Strain 0.200 % |
|
Haynes HR-160® alloy, solution annealed sheet Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Tensile Strength, Yield | 353 MPa @Strain 0.200 % |
51200 psi @Strain 0.200 % |
|
Haynes HR-160® alloy plate, aged 8000 hours at 649°C (1200°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |