Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 352 MPa @Temperature 23.9 °C |
51000 psi @Temperature 75.0 °F |
0° Direction, Dry; 18oz. Woven roving form; ASTM D638 |
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, Glass Reinforced Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel.. |
|||
Tensile Strength, Yield | 352 MPa @Strain 0.200 % |
51000 psi @Strain 0.200 % |
|
Special Metals INCONEL® 690 Nickel Superalloy, Hot Rolled Flat, 0.5 x 2.0 inch (13 x 51 mm) Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and yield) and elongation values reported here are typical for Hot Rolled Flat, 0.5 x 2.. |
|||
Tensile Strength, Yield | >= 352 MPa | >= 51000 psi | 0.2% offset |
Eagle Brass 110 EPT COPPER, Extra Spring Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of .. |
|||
Tensile Strength, Yield | 352 - 407 MPa | 51000 - 59000 psi | 0.2% offset |
Eagle Brass 151 ZHC® COPPER, Hard Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c.. |
|||
Tensile Strength, Yield | 352 - 414 MPa | 51000 - 60000 psi | 0.2% offset |
Eagle Brass 230 Red Brass, 3/4 Hard CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste.. |
|||
Tensile Strength, Yield | 352 - 455 MPa | 51000 - 66000 psi | 0.2% offset |
Eagle Brass 425 Tin Brass 2%, 1/2 Hard Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Tensile Strength, Yield | 352 - 517 MPa | 51000 - 75000 psi | 0.2% offset |
Eagle Brass 521 Phosphor Bronzes 8% C, 1/2 Hard Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Tensile Strength, Yield | >= 352 MPa | >= 51000 psi | 0.2% offset |
Eagle Brass 101 OFE COPPER (Certified), Extra Spring Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information.. |
|||
Tensile Strength, Yield | >= 352 MPa | >= 51000 psi | 0.2% offset |
Eagle Brass 102 OF COPPER (Non-Certified), Extra Spring Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an.. |