Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 3.45 MPa | 500 psi | at 200%, as molded |
Multibase SILASTIC® C7-4565 VAROX Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 3.45 MPa | 500 psi | ASTM D412 |
Polymax® Maxelast® P3935T TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 3.45 MPa | 500 psi | at 100%; ASTM D412 |
MF-5062 Polyurethane-based Biomedical Elastomer |
|||
Tensile Strength, Yield | 3.45 - 34.5 MPa | 500 - 5000 psi | Average value: 24.1 MPa Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "ABS + Glass Blend". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Tensile Strength, Yield | 3.45 MPa | 500 psi | at 100%; ASTM D412 |
Multibase Multi-Flex® A 7005 C TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Tensile Strength, Yield | 3.45 MPa | 500 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® A 8030 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Tensile Strength, Yield | 3.45 MPa | 500 psi | AVG Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 7267 Ethylene-Propylene Rubber EPDM for high temperature steam service. Also available as a Y267-Type (7267L).Information provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 3.45 MPa | 500 psi | ASTM D638 |
Techmer ES HiFill® ABS GB10 10% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 3.45 MPa | 500 psi | 100%; ASTM D412 |
Teknor Apex APEX® 2560-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin.. |
|||
Tensile Strength, Yield | 3.45 MPa @Strain 300 % |
500 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP 9000 Thermoplastic Elastomer Notes: Translucent Features: High FlowInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 3.45 MPa @Strain 300 % |
500 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP 1304S Thermoplastic Elastomer Uses: Grips Features: Good Resistance to Skin OilsInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 3.45 MPa | 500 psi | ASTM D412 |
Teknor Apex TEKBOND® 6700-35 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 3.45 MPa | 500 psi | ISO 527 |
A. Schulman SCHULAMID® 6 NV12 Easy Flow Low Viscosity Nylon 6 Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 3.45 MPa | 500 psi | ISO 527 |
A. Schulman SCHULAMID® 6 NV12 Easy Flow Low Viscosity Nylon 6 Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 3.45 MPa | 500 psi | ISO 527 |
A. Schulman SCHULAMID® 6 NV12 Easy Flow Low Viscosity Nylon 6 Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 3.45 MPa | 500 psi | ISO 527 |
A. Schulman SCHULAMID® 6 NV12 Easy Flow Low Viscosity Nylon 6 Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 3.45 MPa | 500 psi | ISO 527 |
A. Schulman SCHULAMID® 6 NV12 Easy Flow Low Viscosity Nylon 6 Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 3.45 MPa @Strain <=1.00 % |
500 psi @Strain <=1.00 % |
Silicone Property; Arlon SQA-TMS-008 |
Arlon Thermabond® 99A30N008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier.. |
|||
Tensile Strength, Yield | 3.45 MPa @Strain <=1.00 % |
500 psi @Strain <=1.00 % |
Silicone Property; Arlon SQA-TMS-008 |
Arlon Thermabond® R37260N008 0.008" Uncured Silicone Rubber on Fiberglass Carrier Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction:Liner: 1 mil FEPProduct: Uncured Silicone RubberCarrier: 3 m.. |
|||
Tensile Strength, Yield | 3.45 MPa | 500 psi | cured 7 mins @ 150°C |
ACC QSil 550R QSI Quantum Silicones Silicone Potting Material QSil 550Ris a 100% silicone solids elastomer designed for electronic potting applications. The two-component system offers a hard, thermally conductive, low modulus material that is readily repairab.. |
|||
Tensile Strength, Yield | 3.45 MPa | 500 psi | cured 20 mins @ 150°C |
ACC QSil 550SB QSI Quantum Silicones Self-Priming Silicone Potting Material QSil 550SB is a 100% silicone solids elastomer designed for electronic potting applications. The two-component system offers a hard, thermally conductive, low modulus material that is readily repair.. |
|||
Tensile Strength, Yield | 3.45 MPa | 500 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® A 6221 CUV A Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Tensile Strength, Yield | 3.45 - 100 MPa | 500 - 14500 psi | Average value: 63.2 MPa Grade Count:310 |
Overview of materials for Nylon 6, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Tensile Strength, Yield | 3.45 MPa | 500 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® RT-3730 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledNaturalApplications:General PurposeMarket:Consumer GoodsIndustrialBuilding and ConstructionProcessing Method:Injection Molding.. |
|||
Tensile Strength, Yield | 3.45 MPa @Strain 300 % |
500 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® RT-5165 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerNaturalIgnition ResistantApplications:Multi-PurposeMarket:Building and ConstructionConsumer GoodsIndustrialProcessing Method:Injection Mo.. |
|||
Tensile Strength, Yield | 3.45 MPa | 500 psi | TM R050-36 |
Resinlab® EP1240RC Flame Retardant Epoxy Casting Resin Resinlab™ EP1240RC is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034, Pro.. |
|||
Tensile Strength, Yield | 3.45 MPa | 500 psi | at 100%; ASTM D412 |
MF-5056 Polyurethane-based Biomedical Elastomer |