Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 3.38 MPa | 490 psi | 200%, post cured- 4 hours at 204°C |
Multibase SILASTIC® C7-4550 TBPB Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 3.38 MPa @Strain 100 % |
490 psi @Strain 100 % |
across flow; ASTM D412 |
ExxonMobil Santoprene® 121-80M300 Thermoplastic Rubber
(discontinued **) Description: A black thermoplastic high-flow elastomer for excellent injection molding performance with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloropren.. |
|||
Tensile Strength, Yield | 3.38 MPa | 490 psi | ASTM D638 |
ExxonMobil OPTEMA™ TC 130 Molding, extrusion and compounding resin
(discontinued **) OPTEMA TC 130 is an ethylene methyl acrylate copolymer, which can be used in specialty applications such as a carrier for color and additive master batches, a compatibilizer in polymer compounds and.. |
|||
Tensile Strength, Yield | 3.38 MPa | 490 psi | 200%, post cured- 4 hours at 177°C; ASTM D412 |
Multibase C6-250 VAROX DBPH Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 3.38 MPa | 490 psi | ASTM D412 |
Elastocon TPE Technologies Elastocon® 8038N Thermoplastic Elastomer Elastocon® 8038N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8038N is FDA compliant and well suited.. |
|||
Tensile Strength, Yield | 3.38 MPa | 490 psi | 2.0 in/min; ASTM D638 |
ExxonMobil PP4712E1 Polymer Grade for Oriented Film Product Description: Easy processing grade primarily for oriented film applications.Availability: North America and South America Features:MetalizableUses: Industrial Applications Oriented FilmTo.. |
|||
Tensile Strength, Yield | 3.38 - 42.1 MPa | 490 - 6110 psi | Average value: 32.7 MPa Grade Count:130 |
Overview of materials for Polypropylene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr.. |