Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 33.3 MPa | 4840 psi | ASTM D638 |
Hyosung Topilene HJ640 PP HJ640 High Isostatic PP Impact CopolymerApplications:CompoundingElectric applianceAutomobile partsCharacteristics:High stiffnessHeat resistanceMedium impactInformation provided by Hyosung Corporatio.. |
|||
Tensile Strength, Yield | 33.3 MPa @Thickness 3.20 mm |
4840 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUPOL HG3100 PP+MF10%, High Gloss Description: Injection Molding, PP+MF10%, High GlossApplication: Electrical & Electronic PartsCAS: 9003-07-0 and 7727-43-7Information provided by LG Chemical |
|||
Tensile Strength, Yield | 33.3 MPa @Thickness 3.20 mm |
4840 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUPOL GP3400 PP+MF40% Description: Injection Molding, PP+MF30%, General PurposeApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Tensile Strength, Yield | 33.3 MPa @Thickness 3.20 mm |
4840 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUPOL GP3400S PP+MF40% Description: Injection Molding, PP+MF40%, General Purpose, Low WarpageApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 12001-26-2Information provided by LG Chemica.. |
|||
Tensile Strength, Yield | 33.3 MPa | 4840 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-0852 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 33.3 MPa | 4840 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-0852 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 33.3 MPa | 4840 psi | ASTM D638 |
Cheng Yu Plastic PP230H TALC 30 Polypropylene, 30% Talc, High Heat |
|||
Tensile Strength, Yield | 33.4 MPa | 4840 psi | ISO 527-2/50 |
ExxonMobil Exxtral™ HMU 301 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for high heat and discoloration resistance, good surface finish, and detergent resistance for electrical appliances such as w.. |
|||
Tensile Strength, Yield | 33.4 MPa | 4840 psi | at elastic yield; ASTM D412 |
Clariant Renol PURSP0002 Polyurethane Elastomer, Ether Based Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 33.3 MPa | 4840 psi | |
Zylog Hipolyene® 8021 HC Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |