Polymer Property : Tensile Strength, Yield = 4601 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.72 MPa
4601 psi
ASTM D638
Lucent Polymers TPP-130 Polypropylene, Homopolymer, 30% Talc Filled
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.