Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 2.50 - 28.3 MPa | 363 - 4110 psi | Average value: 7.13 MPa Grade Count:24 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum .. |
|||
Tensile Strength, Yield | >= 2.50 MPa | >= 363 psi | |
Trelleborg Offshore Vikotherm™ 73961 Insulative Elastomer Vikotherm™ is a rubber elastomer chemically modified to provide very high insulating characteristics while maintaining its inherent rubber properties in respect of seawater resistance, pressure res.. |
|||
Tensile Strength, Yield | >= 2.50 MPa | >= 363 psi | |
Trelleborg Offshore Vikotherm™ 73982 Insulative Elastomer Vikotherm™ is a rubber elastomer chemically modified to provide very high insulating characteristics while maintaining its inherent rubber properties in respect of seawater resistance, pressure res.. |
|||
Tensile Strength, Yield | 2.50 MPa @Strain 100 % |
363 psi @Strain 100 % |
ISO 527-1/-2 |
Covestro Desmopan® DP 1960AW Polyurethane As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Tensile Strength, Yield | 2.50 MPa @Strain 100 % |
363 psi @Strain 100 % |
ISO 527-1/-2 |
Covestro Desmopan® DP 1966AW Polyurethane As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Tensile Strength, Yield | 2.50 MPa @Strain 100 % |
363 psi @Strain 100 % |
ISO 527-1/-2 |
Covestro Desmopan® DP 3070AU Polyurethane injection molding gradefree from plasticizersApplicationInjection molded engineering partshard - soft systemsAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially .. |
|||
Tensile Strength, Yield | 2.50 MPa | 363 psi | |
Dow AFFINITY™ SM 8250 Polyolefin Plastomer AFFINITY® SM 8250 polyolefin plastomer is an alpha-olefin resin that offers excellent performance in injection molded clear or colored flexible durable parts. It exhibits excellent clarity and flex.. |
|||
Tensile Strength, Yield | 2.50 MPa | 363 psi | 508 mm/min; ASTM D638 |
Dow Engage® 8452 Polyolefin Elastomer Description: Engage® 8452 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent toughness, softness, and optical properties. It has excellent compatibility with other polyolefin.. |
|||
Tensile Strength, Yield | 2.50 MPa | 363 psi | |
ACC MM282 Specialist Molding 2-Part Condensation Cure Part of the Amber Chemical Group. Data provided by manufacturer. |
|||
Tensile Strength, Yield | 2.50 MPa | 363 psi | |
ACC MM911 Condensation Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: high tear strength, picks up extremely fine details, low viscosity, good resistance to styrene attack, easy degassing.. |
|||
Tensile Strength, Yield | 2.50 MPa | 363 psi | 50 mm/min |
Arkema Group Evatane® 1350 VN 5 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for molding very flexible articles. Examples: gaskets.ISO data provided by the manufacturer, Arkema. |