Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 22.1 MPa | 3210 psi | ASTM D638 |
ExxonMobil Escorene® HD-6733 HDPE, Injection Grade
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: High Flow, Good StiffnessUses: Food containers, Small pails, Nursery containers |
|||
Tensile Strength, Yield | 22.1 - 59.3 MPa @Temperature -18.0 - 71.0 °C |
3210 - 8600 psi @Temperature -0.400 - 160 °F |
Average value: 40.7 MPa Grade Count:1 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Tensile Strength, Yield | 22.1 MPa | 3210 psi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 6 PHR Varox DBPH-50 MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 22.1 MPa | 3210 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Propionate CP800 (Base Grade), 18% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Tensile Strength, Yield | 22.1 MPa | 3210 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Propionate CP801 (UV Inhibitor Added), 18% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Tensile Strength, Yield | 22.1 MPa | 3210 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Propionate CP808 (FDA), 18% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Tensile Strength, Yield | 22.1 MPa | 3210 psi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 6 PHR Varox DBPH-50 MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 22.1 MPa | 3210 psi | ASTM D638 |
Eastman Tenite 307A4000018 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Tensile Strength, Yield | 22.1 MPa | 3210 psi | ASTM D638 |
Eastman Tenite 307E4000018 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Tensile Strength, Yield | 22.1 MPa | 3210 psi | ASTM D638 |
Eastman Tenite 380A3V32818 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Tensile Strength, Yield | 22.1 MPa | 3210 psi | ASTM D638 |
Eastman Tenite Propionate 307A2R30018 Natural, Trsp Cellulose Acetate Propionate Plasticizer 18%. Weight loss on heating = 1% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pro.. |
|||
Tensile Strength, Yield | 22.1 MPa | 3210 psi | ASTM D638 |
Eastman Tenite Propionate 371A2R30012 Natural, Trsp Cellulose Acetate Propionate Plasticizer 18%. Weight loss on heating = 1% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pro.. |
|||
Tensile Strength, Yield | 22.1 MPa | 3210 psi | ASTM D638 |
Eastman Tenite Propionate 380A2R30018 Natural, Trsp Cellulose Acetate Propionate Plasticizer 18%. Weight loss on heating = 1% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pro.. |
|||
Tensile Strength, Yield | 22.1 MPa | 3210 psi | ASTM Data |
Dow AIM® 4900 High Impact Styrenic Resin AIM® 4900 advanced styrenic resin for extrusion and thermoforming applications is designed to offer the processability of high impact polystyrene and the gloss and practical toughness of high gloss.. |
|||
Tensile Strength, Yield | 22.1 MPa | 3210 psi | Molded property |
Dow DOWLEX™ 2027A Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2027A Polyethylene resin is a higher density polymer for cast film applications with improved stiffness. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2(a) for food contact appli.. |
|||
Tensile Strength, Yield | 22.1 MPa | 3210 psi | |
Dow HDPE 30460M High Density Polyethylene DOW HDPE 30460M resin is a medium molecular weight distribution copolymer designed to offer moderate impact strength and stress crack resistance with excellent rigidity. This resin has excellent pro.. |
|||
Tensile Strength, Yield | 22.1 MPa | 3210 psi | ASTM D-638 |
Axiall 15642 Wire & Cable Flexible PVC Non-lead stabilized semi-rigid insulation compound recommended for Style #1061 applications. Maximum service temperature of 105°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Cor.. |
|||
Tensile Strength, Yield | 22.1 MPa | 3210 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable W1100L-xx92FRD Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Tensile Strength, Yield | 22.1 MPa | 3210 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable W1100L-xx92FRDA Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Tensile Strength, Yield | 22.1 - 41.4 MPa | 3210 - 6000 psi | Average value: 30.5 MPa Grade Count:74 |
Overview of materials for Cellulose Acetate Propionate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Propionate, Molded". Each property range of values reported is minimum and maximum val.. |