Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 21.1 MPa | 3060 psi | ASTM D412 |
Precision Polymer Engineering Perlast® G80A Perfluoroelastomer A black general purpose perfluoroelastomer compound with excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties.Applications: Do not use any P.. |
|||
Tensile Strength, Yield | 21.1 MPa @Thickness 3.20 mm |
3060 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOL HF5157Z PP+Rubber+MF, High Flow and Stiffness, High Impact Description: Injection Molding, PP+Rubber+MF, High Flow and Stiffness, High Impact, Good PaintabilityApplication: Automotive Exterior (Slim wall Bumper Fascia)Information provided by LG Chemical |
|||
Tensile Strength, Yield | 21.1 MPa @Temperature 23.0 °C |
3060 psi @Temperature 73.4 °F |
ASTM D638 |
Ineos N20L-00 Polypropylene Impact Copolymer This is a nucleated polypropylene impact copolymer formulated with a slip agent for improved mold release, and has an optimum balance of stiffness and impact resistance for injection molding applica.. |
|||
Tensile Strength, Yield | 21.1 MPa | 3060 psi | |
Spartech M60095 General Purpose PVC First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B.. |
|||
Tensile Strength, Yield | 21.1 MPa | 3060 psi | |
Zylog Hipolyene® 6251 Y M4 C Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Tensile Strength, Yield | 21.1 MPa | 3060 psi | 150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2 |
Solvay Engineered Polymers DEXFLEX® 925 TPO
(discontinued **) Description: DEXFLEX® 925 is a thermoplastic olefinic elastomer (TPO) designed for automotive exterior applications that require a combination of stiffness, low-temperature impact resistance, and e.. |