Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 19.2 MPa | 2780 psi | ASTM D412 |
Precision Polymer Engineering Perlast® G75B High Temperature Perfluoroelastomer Perlast® G75B offers a unique blend of excellent chemical resistance, temperature capabilities and mechanical properties, simultaneously extending the operating limits in all three aspects. Perlas.. |
|||
Tensile Strength, Yield | 19.2 MPa | 2780 psi | 2.0 in/min; ASTM D638 |
ExxonMobil PP8244E1 Polypropylene Homopolymer Product Description: A high crystallinity, high impact copolymer resin designed for injection molded applications requiring excellent processing attributes.Availability: North America Features:Bala.. |